WC-TiC-TaC-Co硬质合金中TaC含量对其显微组织和力学性能的影响
|
|
Effect of TaC Content on Microstructure and Mechanical Properties of WC-TiC-TaC-Co Cemented Carbide
|
|
图3. WC-TiC-TaC-Co硬质合金中WC和(W, Ti, Ta)C晶粒尺寸分布图 |
Fig.3. Grain size distributions of WC (a) and (W, Ti, Ta)C (b) in WC-TiC-TaC-Co cemented carbides |
![]() |