预变形对超高强Al-Zn-Mg-Cu合金时效组织与力学性能的影响
韩宝帅, 魏立军, 徐严谨, 马晓光, 刘雅菲, 侯红亮

Effect of Pre-Deformation on Microstructure and Mechanical Properties of Ultra-High Strength Al-Zn-Mg-Cu Alloy After Ageing Treatment
HAN Baoshuai, WEI Lijun, XU Yanjin, MA Xiaoguang, LIU Yafei, HOU Hongliang
表1 时效工艺参数
Table 1 Ageing process parameters
Sample No.Heat treatment processAbbreviation
1No deformation alloy+80 ℃, 12 h+120 ℃, 8 h12+8
23% deformation alloy+80 ℃, 12 h+120 ℃, 8 h3%+12+8
34% deformation alloy+80 ℃, 12 h+120 ℃, 8 h4%+12+8
4No deformation alloy+80 ℃, 12 h+120 ℃, 10 h12+10