金属Mg二阶锥面<c+a>刃位错运动特性的分子动力学模拟
|
|
Motion Characteristics of <c+a> Edge Dislocation on the Second-Order Pyramidal Plane in Magnesium Simulated by Molecular Dynamics
|
|
图4. 正、负剪切时位错运动速率(v)随 |
Fig.4. Dislocation velocity (v) as a function of |
![]() |