[an error occurred while processing this directive]
温度对碳纳米管增强纳米蜂窝镍力学性能的影响
李源才, 江五贵(), 周宇
Effect of Temperature on Mechanical Propertiesof Carbon Nanotubes-Reinforced Nickel Nano-Honeycombs
LI Yuancai, JIANG Wugui(), ZHOU Yu

图11. 温度为600 K时CRNNHC在径向拉伸、径向压缩、轴向拉伸和轴向压缩变形下的原子分布图

Fig.11. Atomic snapshots of CRNNHC along different deformation directions of radial tension (a, b), radial compression (c, d), axial tension (e, f) and axial compression (g, h) under the temperature of 600 K
(a) εu=0.086 (b) εu=0.586 (c) εu=0.076 (d) εu=0.436
(e) εu=0.090 (f) εu=0.353 (g) εu=0.056 (h) εu=0.096