温度对碳纳米管增强纳米蜂窝镍力学性能的影响
李源才, 江五贵(), 周宇
Effect of Temperature on Mechanical Propertiesof Carbon Nanotubes-Reinforced Nickel Nano-Honeycombs
LI Yuancai, JIANG Wugui(), ZHOU Yu

图9. 不同温度下轴向压缩应力-应变曲线

Fig.9. The axial compression stress-strain curves of NNHC (a) and CRNNHC (b) with different temperatures