温度对碳纳米管增强纳米蜂窝镍力学性能的影响
李源才, 江五贵(), 周宇
Effect of Temperature on Mechanical Propertiesof Carbon Nanotubes-Reinforced Nickel Nano-Honeycombs
LI Yuancai, JIANG Wugui(), ZHOU Yu

图3. 不同温度下NNHC和CRNNHC沿径向拉伸的力学性能

Fig.3. The radial tensile E (a) and σu (b) of NNHC and CRNNHC with different temperatures (E—elastic modulus, σu—ultimate stress)