纳米孔洞对单晶/多晶Ni复合体拉伸性能的影响
李源才, 江五贵(), 周宇
Effect of Nanopores on Tensile Properties of Single Crystal/Polycrystalline Nickel Composites
LI Yuancai, JIANG Wugui(), ZHOU Yu

图7. 不同应变下单晶/多晶Ni复合体径向分布函数(G(r))

Fig.7. Radial distribution function (G(r)) curves of single crystal/polycrystalline nickel composites under different strains (r—distance between atoms)