纳米孔洞对单晶/多晶Ni复合体拉伸性能的影响
李源才, 江五贵(), 周宇
Effect of Nanopores on Tensile Properties of Single Crystal/Polycrystalline Nickel Composites
LI Yuancai, JIANG Wugui(), ZHOU Yu

图2. 无预制孔洞与孔洞半径为1.1 nm时不同晶态Ni应力-应变曲线

Fig.2. Tensile stress-strain curves of different constructions of crystalline nickel with void-free and with a prefabricated void with radius R=1.1 nm