(CoCrFeMnNi)97.02Mo2.98高熵合金σ相析出演变及力学性能
姚小飞(), 魏敬鹏, 吕煜坤, 李田野
Precipitation σ Phase Evoluation and Mechanical Properties of (CoCrFeMnNi)97.02Mo2.98 High Entropy Alloy
YAO Xiaofei(), WEI Jingpeng, LV Yukun, LI Tianye

图4. 不同温度退火热处理后(CoCrFeMnNi)97.02Mo2.98高熵合金的工程应力-应变曲线

Fig.4. The stress-strain curves of (CoCrFeMnNi)97.02-Mo2.98 high entropy alloys after annealing at different temperatures