(CoCrFeMnNi)97.02Mo2.98高熵合金σ相析出演变及力学性能
姚小飞(), 魏敬鹏, 吕煜坤, 李田野
Precipitation σ Phase Evoluation and Mechanical Properties of (CoCrFeMnNi)97.02Mo2.98 High Entropy Alloy
YAO Xiaofei(), WEI Jingpeng, LV Yukun, LI Tianye

图3. 不同温度退火热处理后(CoCrFeMnNi)97.02Mo2.98高熵合金的显微硬度

Fig.3. Microhardness of (CoCrFeMnNi)97.02Mo2.98 high entropy alloys after annealing at different temperatures