[an error occurred while processing this directive]
金刚石工具用Cu-10Sn-xNi合金的制备和性能表征
刘震鹏1,2, 闫志巧2, 陈峰2(), 王顺成2, 龙莹3, 吴益雄4
Fabrication and Performance Characterization of Cu-10Sn-xNi Alloy for Diamond Tools
LIU Zhenpeng1,2, YAN Zhiqiao2, CHEN Feng2(), WANG Shuncheng2, LONG Ying3, WU Yixiong4

图4. 热压烧结Cu-10Sn-xNi合金的BSE像

Fig.4. BSE images of hot pressing sintering Cu-10Sn-xNi alloys with x=15 (a1~a3) , x=30 (b1~b3) , x=45 (c1~c3) and x=60 (d1~d3) at temperatures of 820 ℃ (a1~d1) , 850 ℃ (a2~d2) and 880 ℃ (a3~d3)