氙离子辐照后Hastelloy N合金的纳米硬度及其数值模拟
|
|
Numerical Simulation of Nanohardness in Hastelloy N Alloy After Xenon Ion Irradiation
|
|
图3. 离子辐照前后各个样品的平均纳米硬度随压头压入深度变化的曲线 |
Fig.3. Indentation depth dependence of the average nanohardness of the unirradiated and irradiated samples |
![]() |