氙离子辐照后Hastelloy N合金的纳米硬度及其数值模拟
|
|
Numerical Simulation of Nanohardness in Hastelloy N Alloy After Xenon Ion Irradiation
|
|
图2. 进行纳米压痕实验后试样的压痕形状OM像 |
Fig.2. OM image of indentation shape of sample after nanoindentation experiment |
![]() |