激光沉积薄壁结构热力演化的尺寸效应
王霞1,2, 王维1,2(), 杨光2, 王超2, 任宇航2
Dimensional Effect on Thermo-Mechanical Evolution of Laser Depositing Thin-Walled Structure
WANG Xia1,2, WANG Wei1,2(), YANG Guang2, WANG Chao2, REN Yuhang2

图7. 薄壁长度为30 mm时0.25、3.75和15.875 s 变形分布云图

Fig.7. Distributions of deformation at the time of 0.25 s (a), 3.75 s (b) and 15.875 s (c) when L=30 mm (The deformations are magnified by a factor of 6)