[an error occurred while processing this directive]
激光沉积薄壁结构热力演化的尺寸效应
王霞1,2, 王维1,2(), 杨光2, 王超2, 任宇航2
Dimensional Effect on Thermo-Mechanical Evolution of Laser Depositing Thin-Walled Structure
WANG Xia1,2, WANG Wei1,2(), YANG Guang2, WANG Chao2, REN Yuhang2

图4. 最高温度曲线中沉积段峰值和谷值温度以及最低温度曲线中峰值和终值温度

Fig.4. Peak and valley temperatures of the depositing part on the maximum temperature curves (a), peak and final temperatures of the minimum temperature curves (b)