人工时效对2A12铝板力学性能和强化相的影响
梁孟超, 陈良(), 赵国群
Effects of Artificial Ageing on Mechanical Properties and Precipitation of 2A12 Al Sheet
LIANG Mengchao, CHEN Liang(), ZHAO Guoqun

图8. 沿[001]Al方向Al基体及S相衍射斑点示意图

Fig.8. Schematics of the diffraction spots of Al matrix and S phases along [001]Al direction
(a) Al matrix (b) S phases of [100]S//[100]Al (A and B) or [100]S// [010]Al (C and D) (c) S phases of [100]S//[001]Al