Mg-5.6Gd-0.8Zn合金多向锻造过程中的变形机制及动态再结晶
张阳, 邵建波, 陈韬, 刘楚明, 陈志永()
Deformation Mechanism and Dynamic Recrystallization of Mg-5.6Gd-0.8Zn Alloy During Multi-Directional Forging
ZHANG Yang, SHAO Jianbo, CHEN Tao, LIU Chuming, CHEN Zhiyong()

图8. 合金锻后各道次取向成像图

Fig.8. Orientation maps of multi-directional forged alloy after 1-pass (a), 2-pass (b), 3-pass (c) and 6-pass (d) (Twins with smaller size can be observed in the grains with c-axes near parallel to the forging direction, as marked as ellipses in Fig.8a; with the changing of forging direction, untwined grains in the 1-pass are rotated to the favorable orientation for twinning (<21ˉ1ˉ0> parallel to CD), as indicated by ellipses in Fig.8b)