Mg-5.6Gd-0.8Zn合金多向锻造过程中的变形机制及动态再结晶
张阳, 邵建波, 陈韬, 刘楚明, 陈志永()
Deformation Mechanism and Dynamic Recrystallization of Mg-5.6Gd-0.8Zn Alloy During Multi-Directional Forging
ZHANG Yang, SHAO Jianbo, CHEN Tao, LIU Chuming, CHEN Zhiyong()

图3. 退火态合金长周期堆垛结构(LPSO)相的STEM像

Fig.3. STEM image and selected area electron diffraction (SAED) pattern (a) and magnification of the LPSO phase as marked in Fig.3a (b) (Beam direction is <112ˉ0>)