[an error occurred while processing this directive]
Mg-5.6Gd-0.8Zn合金多向锻造过程中的变形机制及动态再结晶
张阳, 邵建波, 陈韬, 刘楚明, 陈志永()
Deformation Mechanism and Dynamic Recrystallization of Mg-5.6Gd-0.8Zn Alloy During Multi-Directional Forging
ZHANG Yang, SHAO Jianbo, CHEN Tao, LIU Chuming, CHEN Zhiyong()

图2. 铸态、均匀化态及退火态Mg-5.6Gd-0.8Zn合金的SEM像

Fig.2. SEM images of as-cast (a), homogenized (b) and annealed (c, d) Mg-5.6Gd-0.8Zn alloy before multi-directional forging (The lamellar second phases are indicated by black arrows in Fig.2d, LPSO—long-period stacking ordered)