Fe-15Mn-5Si-14Cr-0.2C非晶钢微观组织与腐蚀行为
赵燕春1,2(), 毛雪晶1, 李文生1, 孙浩1, 李春玲3, 赵鹏彪1, 寇生中1
Microstructure and Corrosion Behavior of Fe-15Mn-5Si-14Cr-0.2C Amorphous Steel
ZHAO Yanchun1,2(), MAO Xuejing1, LI Wensheng1, SUN Hao1, LI Chunling3, ZHAO Pengbiao1, KOU Shengzhong1, Liaw Peter K.2

图1. Fe-15Mn-5Si-14Cr-0.2C铸态和加载断裂后试样XRD谱

Fig.1. XRD spectra of as-cast Fe-15Mn-5Si-14Cr-0.2C sample and fractured sample after loading