Fe-15Mn-5Si-14Cr-0.2C非晶钢微观组织与腐蚀行为 |
||||||||||||||||||
| 赵燕春, 毛雪晶, 李文生, 孙浩, 李春玲, 赵鹏彪, 寇生中 | ||||||||||||||||||
|
Microstructure and Corrosion Behavior of Fe-15Mn-5Si-14Cr-0.2C Amorphous Steel |
||||||||||||||||||
| ZHAO Yanchun, MAO Xuejing, LI Wensheng, SUN Hao, LI Chunling, ZHAO Pengbiao, KOU Shengzhong, Liaw Peter K. | ||||||||||||||||||
| 表2 Fe-15Mn-5Si-14Cr-0.2C合金腐蚀后边缘区域和中心区域的EDS分析结果 (mass fraction / %) |
||||||||||||||||||
| Table 2 EDS analyses of Fe-15Mn-5Si-14Cr-0.2C alloy after electrochemical corrosion at margin and center areas |
||||||||||||||||||
|
||||||||||||||||||