基于
Ce
变质处理的
TWIP
钢凝固组织细化
李根, 兰鹏(
), 张家泉
Solidification Structure Refinement in TWIP Steel by Ce Inoculation
LI Gen, LAN Peng(
), ZHANG Jiaquan
图11.
Ce含量对TWIP钢试样Mn元素偏析比的影响
Fig.11.
Effects of Ce content on Mn segregation ratio of TWIP steel