基于Ce变质处理的TWIP钢凝固组织细化
李根, 兰鹏(), 张家泉
Solidification Structure Refinement in TWIP Steel by Ce Inoculation
LI Gen, LAN Peng(), ZHANG Jiaquan

图5. Ce含量对TWIP钢试样CET位置与表面距离及等轴晶率的影响

Fig.5. Effects of Ce content on the distance of CET position from surface (a) and the ratio of equiaxed grain area (b) of TWIP steel