选区激光熔化316L不锈钢的拉伸性能
余晨帆1, 赵聪聪1, 张哲峰2, 刘伟1()
Tensile Properties of Selective Laser Melted 316L Stainless Steel
YU Chenfan1, ZHAO Congcong1, ZHANG Zhefeng2, LIU Wei1()

图4. 选区激光熔化316L不锈钢拉伸工程应力-应变曲线

Fig.4. Tensile engineering stress-strain curves of 316L stainless steel fabricated by SLM