[an error occurred while processing this directive]
冷变形和固溶温度对HR3C钢中σ相析出行为的影响
曹铁山1,2, 赵津艺1, 程从前1, 孟宪明3, 赵杰1()
Effect of Cold Deformation and Solid Solution Temperature on σ-phase Precipitation Behavior in HR3C Heat Resistant Steel
CAO Tieshan1,2, ZHAO Jinyi1, CHENG Congqian1, MENG Xianming3, ZHAO Jie1()

图7. 不同冷变形的HR3C钢在750 ℃时效时σ相体积分数随时间的变化关系

Fig.7. Volume fraction of σ phase versus time for HR3C steel ageing at 750 ℃