冷变形和固溶温度对HR3C钢中σ相析出行为的影响
曹铁山1,2, 赵津艺1, 程从前1, 孟宪明3, 赵杰1()
Effect of Cold Deformation and Solid Solution Temperature on σ-phase Precipitation Behavior in HR3C Heat Resistant Steel
CAO Tieshan1,2, ZHAO Jinyi1, CHENG Congqian1, MENG Xianming3, ZHAO Jie1()

图1. 不同状态下的HR3C试样显微组织的OM像

Fig.1. OM images of microstructures of HR3C steel at the states of 8% cold deformation (a), 50% cold deformation (b), 8% cold deformation+1093 ℃ solid solution (c) and 50% cold deformation+1093 ℃ solid solution (d)