高钛耐磨钢中TiC析出行为及其对耐磨粒磨损性能的影响
|
|
TiC Precipitation Behavior and Its Effect on Abrasion Resistance of High Titanium Wear-Resistant Steel
|
|
图3. 实验用钢基体组织的SEM和TEM像 |
Fig.3. SEM (a~c) and TEM images (d, e) of matrix microstructure of tested steels(a) Ti0 (b) Ti20 (c) Ti60(d) Ti0 (e) Ti20 |
![]() |