高钛耐磨钢中TiC析出行为及其对耐磨粒磨损性能的影响
|
|
TiC Precipitation Behavior and Its Effect on Abrasion Resistance of High Titanium Wear-Resistant Steel
|
|
图9. Ti60钢中纳米级TiC粒子的TEM像 |
Fig.9. TEM image of nano-sized TiC particles in Ti60 steel |
![]() |