高钛耐磨钢中TiC析出行为及其对耐磨粒磨损性能的影响
|
|
TiC Precipitation Behavior and Its Effect on Abrasion Resistance of High Titanium Wear-Resistant Steel
|
|
图4. 实验用钢电解萃取析出相粉末的XRD谱 |
Fig.4. XRD spectra of precipitate powder obtained by electrolytic extraction of tested steels |
![]() |