铁素体-贝氏体/马氏体双相钢中界面的定量化晶体学表征
|
|
Quantitative Crystallographic Characterization of Boundaries in Ferrite-Bainite/Martensite Dual-Phase Steels
|
|
图2. 2种实验用钢的低倍EBSD像及整体取向差5°以上界面(红线)分布图 |
Fig.2. Low magnification EBSD maps and grain boundaries with overall misorientation angle above 5° (red lines) of DQ810 (a) and AC730 (b) steelsColor online |
![]() |