高强度含N节Ni奥氏体不锈钢08Cr19Mn6Ni3Cu2N (QN1803)的显微组织及性能 |
||||||||||||||||||
| 蒋一,程满浪,姜海洪,周庆龙,姜美雪,江来珠,蒋益明 | ||||||||||||||||||
|
Microstructure and Properties of 08Cr19Mn6Ni3Cu2N (QN1803) High Strength Nitrogen Alloyed LowNickel Austenitic Stainless Steel |
||||||||||||||||||
| Yi JIANG,Manlang CHENG,Haihong JIANG,Qinglong ZHOU,Meixue JIANG,Laizhu JIANG,Yiming JIANG | ||||||||||||||||||
| 表2 QN1803和S30408钢的室温力学性能 | ||||||||||||||||||
| Table 2 Mechanical properties of QN1803 and S30408 steels at room temperature | ||||||||||||||||||
|
||||||||||||||||||