高强度含N节Ni奥氏体不锈钢08Cr19Mn6Ni3Cu2N (QN1803)的显微组织及性能
|
|
Microstructure and Properties of 08Cr19Mn6Ni3Cu2N (QN1803) High Strength Nitrogen Alloyed LowNickel Austenitic Stainless Steel
|
|
图16. QN1803和S30408钢经5%H2SO4溶液腐蚀6 h后表面形貌的EPMA像 |
Fig.16. EPMA images of surface of QN1803 (a) and S30408 (b) steels corroded in 5%H2SO4 for 6 h |
![]() |