高强度含N节Ni奥氏体不锈钢08Cr19Mn6Ni3Cu2N (QN1803)的显微组织及性能
|
|
Microstructure and Properties of 08Cr19Mn6Ni3Cu2N (QN1803) High Strength Nitrogen Alloyed LowNickel Austenitic Stainless Steel
|
|
图15. QN1803和S30408不锈钢的极化曲线对比 |
Fig.15. Comparisons of polarization curves between QN1803 and S30408 steels |
![]() |