高强度含N节Ni奥氏体不锈钢08Cr19Mn6Ni3Cu2N (QN1803)的显微组织及性能
|
|
Microstructure and Properties of 08Cr19Mn6Ni3Cu2N (QN1803) High Strength Nitrogen Alloyed LowNickel Austenitic Stainless Steel
|
|
图13. QN1803和S30408钢表层合金元素分布 |
Fig.13. Distributions of the alloying elements in the surface of QN1803 (a) and S30408 (b) steels |
![]() |