高强度含N节Ni奥氏体不锈钢08Cr19Mn6Ni3Cu2N (QN1803)的显微组织及性能
|
|
Microstructure and Properties of 08Cr19Mn6Ni3Cu2N (QN1803) High Strength Nitrogen Alloyed LowNickel Austenitic Stainless Steel
|
|
图5. QN1803和S30408钢不同温度下力学性能对比 |
Fig.5. Comparisons of mechanical properties of QN1803 and S30408 steels at different temperatures(a) yield strength (b) tensile strength |
![]() |