高强度含N节Ni奥氏体不锈钢08Cr19Mn6Ni3Cu2N (QN1803)的显微组织及性能
|
|
Microstructure and Properties of 08Cr19Mn6Ni3Cu2N (QN1803) High Strength Nitrogen Alloyed LowNickel Austenitic Stainless Steel
|
|
图3. 固溶温度对QN1803和S30408钢晶粒尺寸的影响 |
Fig.3. Effects of solution temperature on grain size of QN1803 and S30408 steels(a) grain size (b) difference of grain size between QN1803 steel and S30408 steel |
![]() |