[an error occurred while processing this directive]
电磁冶金技术研究新进展
任忠鸣1,2(),雷作胜1,2,李传军1,2,玄伟东1,2,钟云波1,2,李喜1,2
New Study and Development on Electromagnetic Field Technology in Metallurgical Processes
REN Zhongming1,2(),LEI Zuosheng1,2,LI Chuanjun1,2,XUAN Weidong1,2,ZHONG Yunbo1,2,LI Xi1,2

图12. 磁场下纯Al和Bi凝固时的DTA曲线[52,53]

Fig.12. The DTA results of pure Al (a) and Bi (b) at the cooling rate of -5 ℃/min in various magnetic fields, respectively[52,53] (Tn—nucleation temperature)Color online