电磁冶金技术研究新进展
任忠鸣1,2(),雷作胜1,2,李传军1,2,玄伟东1,2,钟云波1,2,李喜1,2
New Study and Development on Electromagnetic Field Technology in Metallurgical Processes
REN Zhongming1,2(),LEI Zuosheng1,2,LI Chuanjun1,2,XUAN Weidong1,2,ZHONG Yunbo1,2,LI Xi1,2

图4. 不同旋转速度下钢液在中间包中的平均停留时间

Fig.4. Influence of the rotation rate on the station time of liquid steel in the tundish