[an error occurred while processing this directive]
电磁冶金技术研究新进展
任忠鸣1,2(),雷作胜1,2,李传军1,2,玄伟东1,2,钟云波1,2,李喜1,2
New Study and Development on Electromagnetic Field Technology in Metallurgical Processes
REN Zhongming1,2(),LEI Zuosheng1,2,LI Chuanjun1,2,XUAN Weidong1,2,ZHONG Yunbo1,2,LI Xi1,2

图1. 施加电磁力时金属熔体中夹杂物上的受力情况示意图[3]

Fig.1. Schematic of the forces on the particle in the melt with imposing electromagnetic force[3] (EMF—electromagnetic force, B—magnetic induction, J—current density)