[an error occurred while processing this directive]
钢的高性能化理论与技术进展
董瀚1,2(),廉心桐1,胡春东1,陆恒昌1,彭伟1,赵洪山1,徐德祥1
High Performance Steels: the Scenario of Theoryand Technology
DONG Han1,2(),LIAN Xintong1,HU Chundong1,LU Hengchang1,PENG Wei1,ZHAO Hongshan1,XU Dexiang1

图20. 6Cr16MoMA马氏体不锈钢SEM像和不同高碳马氏体不锈钢不同奥氏体化温度处理后试样冲击功

Fig.20. SEM image of 6Cr16MoMA martensitic stainless steel (a) and the impact energies of different high carbon martensitic stainless steels after different austenitizing treatments (b) (MA—microalloying)