钢的高性能化理论与技术进展
|
|
High Performance Steels: the Scenario of Theoryand Technology
|
|
图18. 不同高碳马氏体不锈钢的点蚀阻抗谱和腐蚀速率。 |
Fig.18. Nyquist diagrams (a) and corrosion rates (b) of different high carbon contents martensitic stainless steels |
![]() |