钢的高性能化理论与技术进展
董瀚1,2(),廉心桐1,胡春东1,陆恒昌1,彭伟1,赵洪山1,徐德祥1
High Performance Steels: the Scenario of Theoryand Technology
DONG Han1,2(),LIAN Xintong1,HU Chundong1,LU Hengchang1,PENG Wei1,ZHAO Hongshan1,XU Dexiang1

图14. 冷轧和固溶处理05Cr21Mn16Ni2N钢的工程应力-应变曲线

Fig.14. Engineering stress-strain curves of cold rolled and solid solution treated 05Cr21Mn16Ni2N steel