钢的高性能化理论与技术进展
|
|
High Performance Steels: the Scenario of Theoryand Technology
|
|
图3. 添加稀土前后的Q235和09CuPCrNi钢周期浸润腐蚀144 h后的样品形貌及腐蚀速率 |
Fig.3. Corrosion morphologies after dry-wet cycle test for 144 h (a) and corrosion rate during immersion test (b) |
![]() |