钢的高性能化理论与技术进展
|
|
董瀚,廉心桐,胡春东,陆恒昌,彭伟,赵洪山,徐德祥
|
High Performance Steels: the Scenario of Theoryand Technology
|
|
Han DONG,Xintong LIAN,Chundong HU,Hengchang LU,Wei PENG,Hongshan ZHAO,Dexiang XU
|
|
| 表5 我国与日本非调质钢主要成分对比 (mass fraction / %) |
| Table 5 Comparisons of non-quenched and tempered steels between China and Japan |
|
| Country | Code | C | Si | Mn | V | Nb | Cr | Others |
|---|
| China | MFT8 | 0.16~0.26 | ≤0.30 | 1.20~1.60 | ≤0.08 | ≤0.10 | - | - | | MFT9 | 0.18~0.26 | ≤0.30 | 1.20~1.60 | ≤0.08 | ≤0.10 | - | - | | MFT10 | 0.08~0.14 | 0.20~0.35 | 1.90~2.30 | ≤0.10 | ≤0.20 | - | - | | Japan | KNCH7 | 0.19~0.25 | 0.15~0.30 | 1.35~1.65 | - | - | - | - | | (KOBELCO) | KNCH7s | 0.19~0.25 | ≤0.10 | 1.20~1.50 | - | - | - | - | | KNCH8 | 0.27~0.33 | 0.15~0.30 | 1.35~1.65 | - | - | - | - | | KNCH8s | 0.27~0.33 | ≤0.10 | 1.35~1.65 | - | - | - | - | | KNCH8P | 0.12~0.18 | ≤0.10 | 1.35~1.65 | Addition | Addition | - | - | | KNCH9P | 0.19~0.25 | ≤0.10 | 1.35~1.65 | Addition | - | 0.20~0.40 | - | | KNCH10 | 0.37~0.43 | 0.15~0.35 | 1.00~1.30 | Addition | - | - | - | | KNCH12P | 0.15~0.20 | 0.40~0.50 | 1.00~1.30 | Addition | - | 1.20~1.40 | Ti, B, Mo |
|
|
|