630~700 ℃超超临界燃煤电站耐热管及其制造技术进展
|
|
刘正东,陈正宗,何西扣,包汉生
|
Systematical Innovation of Heat Resistant Materials Used for 630~700 ℃ Advanced Ultra-Supercritical (A-USC)Fossil Fired Boilers
|
|
Zhengdong LIU,Zhengzong CHEN,Xikou HE,Hansheng BAO
|
|
| 表2 Inconel617、Inconel617B、C-HRA-3®和C-HRA-2®合金的化学成分[21,22] (mass fraction / %) |
| Table 2 The chemical compositions of Inconel617, Inconel617B, C-HRA-3® and C-HRA-2® alloys[21,22] |
|
| Alloy | Cr | Co | Mo | Al | Ti | C | B | Nb | V | Zr | W | Ni | Ref. |
|---|
| Inconel617 | 20.0~24.0 | 10.0~15.0 | 8.0~10.0 | 0.8~1.5 | ≤0.6 | 0.05~0.15 | ≤0.006 | - | - | - | - | Bal. | ASME SB 167 | | Inconel617B | 21.0~23.0 | 11.0~13.0 | 8.0~10.0 | 0.8~1.3 | 0.25~0.50 | 0.05~0.08 | 0.001~0.005 | ≤0.6 | ≤0.6 | - | - | Bal. | DIN 2.4673 | | C-HRA-3? | 21.0~23.0 | 11.0~13.0 | 8.5~9.0 | 0.8~1.3 | 0.3~0.5 | 0.05~0.08 | 0.002~0.005 | ≤0.1 | ≤0.1 | ≤0.10 | ≤1.0 | Bal. | [21] | | C-HRA-2? | 21.0~23.0 | 11.0~13.0 | 8.5~9.0 | - | - | 0.05~0.08 | 0.002~0.005 | ≤0.1 | - | ≤0.10 | ≤1.0 | Bal. | [22] |
|
|
|