630~700 ℃超超临界燃煤电站耐热管及其制造技术进展
刘正东(),陈正宗,何西扣,包汉生
Systematical Innovation of Heat Resistant Materials Used for 630~700 ℃ Advanced Ultra-Supercritical (A-USC)Fossil Fired Boilers
LIU Zhengdong(),CHEN Zhengzong,HE Xikou,BAO Hansheng

图10. Inconel740H合金胞状碳化物的形貌、SAED谱及TEM像

Fig.10. SEM (a) and TEM (b) images of cellular carbide in Inconel740H alloy, SAED patterns of cellular precipitates and matrix (c) and TEM image of cellular/matrix interface marked by circle in Fig.10b (d)