630~700 ℃超超临界燃煤电站耐热管及其制造技术进展
刘正东(),陈正宗,何西扣,包汉生
Systematical Innovation of Heat Resistant Materials Used for 630~700 ℃ Advanced Ultra-Supercritical (A-USC)Fossil Fired Boilers
LIU Zhengdong(),CHEN Zhengzong,HE Xikou,BAO Hansheng

图4. G115?和P92钢在650 ℃的抗蒸汽腐蚀性能

Fig.4. Comparisions of oxidation resistances of G115? (a) and P92 (b) steels at 650 ℃