630~700 ℃超超临界燃煤电站耐热管及其制造技术进展
刘正东(),陈正宗,何西扣,包汉生
Systematical Innovation of Heat Resistant Materials Used for 630~700 ℃ Advanced Ultra-Supercritical (A-USC)Fossil Fired Boilers
LIU Zhengdong(),CHEN Zhengzong,HE Xikou,BAO Hansheng

图2. G115?钢在650和700 ℃时效过程中M23C6的粗化

Fig.2. M23C6 coarsening of G115? steel during ageing at 650 and 700 ℃