钢铁耐磨材料研究进展
|
|
魏世忠,徐流杰
|
Review on Research Progress of Steel and Iron Wear-Resistant Materials
|
|
Shizhong WEI,Liujie XU
|
|
| 表3 高钒高速钢化学成分[103,104,105,106,107,108] (mass fraction / %) |
| Table 3 chemical compositions of high vanadium high speed steel[103,104,105,106,107,108] |
|
| C | Si | Cr | Mo | W | V | Nb | Fe | Ref. |
|---|
| 1.2~2.6 | <1.0 | 4.0~12.0 | 3.6~6.5 | 3.5~6.5 | 3.5~6.5 | - | Bal. | [103] | | 2.0 | - | 5~7 | 3~4 | 3~4 | 5~6 | - | Bal. | [104] | | 1.6~2.0 | 0.3~1.0 | 4~8 | 4~6 | 1.5~2.5 | 3~5 | 0.5~1.5 | Bal. | [105] | | 2 | - | 5 | 2 | 5 | 8 | - | Bal. | [106] | | 1.4 | 0.26 | 3.92 | 2.83 | 0.75 | 3.34 | | Bal. | [107] | | 2.98 | 0.65 | 4.25 | 2.95 | | 9.80 | | Bal. | [108] |
|
|
|