[an error occurred while processing this directive]
钢铁耐磨材料研究进展
魏世忠1(),徐流杰2()
Review on Research Progress of Steel and Iron Wear-Resistant Materials
WEI Shizhong1(),XU Liujie2()

图10. 滚滑动磨损条件下磨损正切面照片[113]

Fig.10. SEM images of the worn cross-section under rolling sliding wear condition[113](a) high chromium cast iron (Cr20) (b) high-vanadium high-speed steel (V10)